Q-Fog Functions: How it Works

Cyclic corrosion tests expose specimens to a series of different environments in a repetitive cycle. Simple tests may consist of cycling between two conditions: fog and dry. More sophisticated procedures, such as automotive, call for multi-step cycles incorporating humidity or condensation, along with salt fog and dry-off. With the Q-Fog, you can cycle through all these environments in one chamber.  And, with the custom controller, you can easily program complex test cycles or run any of the pre-programmed procedures.

Fog Function

  • During the Fog Function, the corrosion tester typically operates as a conventional salt spray.
  • Corrosive solution from the internal reservoir is pumped to the nozzle.
  • Compressed air is humidified by passing through the bubble tower on its way to the nozzle (except for Prohesion tests).
  • Nozzle atomizes solution air into a corrosive fog.
  • Chamber heaters maintain the programmed chamber temperature.Q-Fog Fog Function

Dry-off Function

  • During the Dry-off Function, a purge blower forces room air over an air heater and into the chamber. This creates a low humidity condition inside the chamber.
  • The chamber temperature is controlled by the chamber heaters and the air heater.Q-Fog Dry Off

Humidity Function

  • During the Humidity Function, the chamber is maintained at 100% relative humidity by forcing hot water vapor into the chamber.
  • The vapor generator heater maintains the programmed chamber temperature.
  • The Humidity Function is available on model CCT only.Q-Fog humidity
 
 
 
 
 
 
 

 

 

 
 
 
 
 
         