Q-Fog testers also feature more precise control of fog volume through the use of a variable speed peristaltic pump. All chambers are constructed of reinforced plastic. There is no internal steel framework to corrode.
| Specification |
SIZE:
|
|
|
Chamber Volume (not including lid) |
18 ftˆ3 511 L |
30.2 ftˆ3 857L |
Chamber Volume (including lid) |
22.6 ftˆ3. 640 L |
38.9 ftˆ3. 1103 L |
Built-in Salt Solution Reservoir |
31.6 gal. 120 L |
31.6 gal. 120 L |
| SAMPLE CAPACITY: |
|
|
4" x 12" Panels (100 x 300 mm) |
128 |
200 |
3" x 6" Panels (75 x 150 mm) |
160 |
240 |
| SAMPLE SPACE: |
|
|
Length |
42.9" 1090 mm |
54.7" 1458 mm |
Width |
25.8" 655 mm |
32.1" 815 mm |
Length (not including lid) |
18" 457 mm |
18" 457 mm |
Length (including lid) |
25.8" 655 mm |
30.5" 755 mm |
| |
|
|
| |
|
|
| |
|
|
|