Now you can supplement your Q-Lab Florida and Arizona test results with additional weathering data from any location you choose. Q-Rack portable outdoor exposure system kits from Q-Lab are versatile, dependable and affordable. They meet ISO, ASTM, SAE and other requirements for outdoor testing. Q-Racks can be shipped to nearly any location in the world. Q-Rack kits, accessories and non-standard mounting systems are available for different applications and testing requirements. The Q-Rack frame may be positioned at 0°, 5°, 45° or 90°. You can adjust capacity with panel flaps or sub-frames. A black box kit that meets SAE J1976 can be added to simulate automotive conditions.
|