Test Standards for Q-PANEL Standard Substrates

ASTM D2201

Standard Practice for Preparation of Zinc-Coated and Zinc-Alloy-Coated Steel Panels for Testing Paint and Related Coating Products

This practice covers the preparation of zinc-coated and zinc-alloy-coated sheet steel panels to be used for testing paint, varnish, lacquer, conversion coatings, and related products.


ASTM D609

Standard Practice for Preparation of Cold-Rolled Steel Panels for Testing Paint, Varnish, Conversion Coatings, and Related Coating Products

This practice covers various types of cold rolled steel panels and the procedures to be followed in their preparation for testing paint, varnish, lacquer, conversion coatings, and related products.


ASTM G50

Standard Practice for Conducting Atmospheric Corrosion Tests on Metals

This practice covers and defines conditions for exposure of metals and alloys to the weather. It sets forth the general procedures that should be followed in any atmospheric test. It is presented as an aid in conducting atmospheric corrosion tests so that some of the pitfalls of such testing may be avoided. As such, it is concerned mainly with panel exposures to obtain data for comparison purposes.


Looking for a specific test standard? Search entire listing of all standards.

 

リソース

コンタクト

  1.  

Q-Lab 電話番号

USA: +1-440-835-8700
Florida と Arizona Test Services: +1-305-245-5600
UK/Europe: +44-1204-861616
Germany: +49-681-857470
China: +86-21-5879-7970

 
View Full Site