ASTM G201

Standard Practice for Conducting Exposures in Outdoor Glass-Covered Exposure Apparatus with Air Circulation

This practice covers the basic principles and operating procedures for using outdoor glass-covered exposure apparatus with air circulation.


Ford DVM0020

Outdoor Weathering Tests

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


GM 2617M

Interior Trim Parts Performance

This specification covers the performance requirements of instrument panels, consoles, door trim, quarter trim panel, garnish moldings, armrests, headrests, assist handles, rear window trim panel and seat trims.


GM 3619M

Flexible Laminating Films and Film Plastic Laminates

This specification details the requirements for flexible plastic films that may be laminated to either metal or plastic substrates.


GM 7454M

Soft Interior Trim Parts

This standard covers the performance and approval requirements for three classes of soft interior trim parts.


GM 7455M

Decorative Interior Plastic Laminates and Films

This specification gives the durability requirements for plastic parts decorated with wood grains, or patterns for interior trim panels. The materials shall be classified into four types.


GM 9538P

Weathering Exposure Tests For Interior Trims

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


GMW 3417

Natural Weathering Exposure Tests for Interior Trims/Materials

This test procedure describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.  The tests are conducted in climatic regions which offer extreme solar environments.


Looking for a specific test standard? Search entire listing of all standards.

 

リソース

コンタクト

  1.  

Q-Lab 電話番号

USA: +1-440-835-8700
Florida と Arizona Test Services: +1-305-245-5600
UK/Europe: +44-1204-861616
Germany: +49-681-857470
China: +86-21-5879-7970

 
View Full Site