Standards

Teste de Exposição Natural Na Flórida

AAMA 2603

Voluntary Specification, Performance Requirements and Test Procedures For Pigmented Organic Coatings on Aluminum Extrusions and Panels

This specification describes test procedures and performance requirements for pigmented organic coatings applied to aluminum extrusions and panels.


AAMA 2605

Voluntary Specification, Performance Requirements and Test Procedures for Superior Performing Organic Coatings on Aluminum Extrusions and Panels

This specification describes test procedures and performance requirements for superior performing organic coatings applied to aluminum extrusions and panels for architectural products.


AATCC TM111

Weather Resistance of Textiles: Exposure to Daylight and Weather

This test method provides a means for determining the weather resistance of textile materials.


ASTM C1589

Standard Practice for Outdoor Weathering of Construction Seals and Sealants

This practice describes outdoor exposure procedures used to determine the weathering durability of building construction, seals and sealants.


ASTM D1006

Standard Practice for Conducting Exterior Exposure Tests of Paints on Wood

This practice covers procedures to be followed for direct exposure of house and trim paints on new, previously unpainted wood materials to the environment.


ASTM D1014

Standard Practice for Conducting Exterior Exposure Tests of Paints and Coatings on Metal Substrates

This practice covers procedures to be followed for direct exposure of exterior paints and coatings to the environment when applied to metal surfaces.


ASTM D1435

Standard Practice for Outdoor Weathering of Plastics

This practice is intended to cover procedures for the exposure of plastic materials to weather. Note 1See Practice G 24 for aging under glass.


ASTM D1670

Standard Test Method for Failure End Point in Accelerated and Outdoor Weathering of Bituminous Materials

This test method covers the use of a spark generating apparatus for determination of failure due to cracking of bituminous materials undergoing accelerated or outdoor weathering on electrically conductive backings.


ASTM D3424

Standard Practice for Evaluating the Relative Lightfastness and Weatherability of Printed Matter

This standard describes procedures for the determination of the relative lightfastness and weatherability of printed matter under the following conditions, which involve exposure to natural daylight or accelerated procedures in the laboratory.


ASTM D3456

Standard Practice for Determining by Exterior Exposure Tests the Susceptibility of Paint Films to Microbiological Attack

This practice provides guidelines for determining the susceptibility of paint films to microbiological attack on exterior exposure. While it is recognized that various organisms may occur on an exposed coating, the specific types of organisms are mainly of academic interest. The degree to which microbiological discoloration occurs is the primary concern.


ASTM D3679

Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Siding

This specification establishes requirements and test methods for the materials, dimensions, warp, shrinkage, impact strength, expansion, appearance, and windload resistance of extruded single-wall siding manufactured from rigid (unplasticized) PVC compound. Methods of indicating compliance with this specification are also provided.


ASTM D4101

Standard Specification for Polypropylene Injection and Extrusion Materials

This specification covers polypropylene materials suitable for injection molding and extrusion. Polymers consist of homopolymer, copolymers, and elastomer compounded with or without the addition of impact modifiers (ethylene-propylene rubber, polyisobutylene rubber, and butyl rubber), colorants, stabilizers, lubricants, or reinforcements.


ASTM D4303

Standard Test Methods for Lightfastness of Colorants Used in Artists' Materials

Four test methods to accelerate the effects of long term indoor illumination on artists' materials are described.


ASTM D4726

Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Exterior-Profile Extrusions Used for Assembled Windows and Doors

This specification establishes requirements for the material properties, including dimensional stability, weatherability, and extrusion quality, of rigid poly(vinyl chloride) (PVC) exterior profile extrusions used for assembled windows and doors.


ASTM D5272

Standard Practice for Outdoor Exposure Testing of Photodegradable Plastics

This practice defines test conditions applicable when Practices D1435 and G7 are employed for the outdoor exposure testing of photodegradable plastics.


ASTM D5819

Standard Guide for Selecting Test Methods for Experimental Evaluation of Geosynthetic Durability

This guide covers a designer/specifier through a systematic determination of those factors of the appropriate application environment that may affect the post-construction service life of a geosynthetic.


ASTM D5970

Standard Test Method for Deterioration of Geotextiles from Outdoor Exposure

This test method covers evaluating the deterioration in tensile strength and strain after outdoor exposure.


ASTM D6551

Standard Practice for Accelerated Weathering of Pressure-Sensitive Tapes by Xenon-Arc Exposure Apparatus

This practice describes one environment for the exposure of pressure-sensitive tape, used primarily for packaging, to a laboratory accelerated weathering environment.


ASTM D6662

Standard Specification for Polyolefin-Based Plastic Lumber Decking Boards

This specification covers polyolefin-based plastic lumber products for use as exterior residential decking boards.


ASTM D6864

Standard Specification for Color and Appearance Retention of Solid Colored Plastic Siding Products

This specification establishes requirements and test methods for the color and appearance retention of solid colored plastic siding products.


ASTM D7251

Standard Specification for Color and Appearance Retention of Variegated Color Plastic Siding Products

This specification establishes requirements and test methods for the color and appearance retention of variegated color plastic siding products.


ASTM D7869

Standard Practice for Xenon Arc Exposure Test with Enhanced Light and Water Exposure for Transportation Coatings

This test procedure is used to simulate the physical and environmental stresses that a coating for exterior transportation applications (for example, automotive) is exposed to in a subtropical climate, such as southern Florida.


ASTM E782

Standard Practice for Exposure of Cover Materials for Solar Collectors to Natural Weathering Under Conditions Simulating Operational Mode

This practice provides a procedure for the exposure of cover materials for flat-plate solar collectors to the natural weather environment at temperatures that are elevated to approximate operating conditions.


ASTM E881

Standard Practice for Exposure of Solar Collector Cover Materials to Natural Weathering Under Conditions Simulating Stagnation Mode

This practice covers a procedure for the exposure of solar collector cover materials to the natural weather environment at elevated temperatures that approximate stagnation conditions in solar collectors having a combined back and edge loss coefficient of less than 1.5 W/(m2 · °C).


ASTM F1164

Standard Test Method for Evaluation of Transparent Plastics Exposed to Accelerated Weathering Combined with Biaxial Stress

This test method covers the resistance of transparent plastics exposed to environmental conditioning (accelerated weathering) under a biaxial stress state induced by a pressure cell/test fixture.


ASTM F1515

Standard Test Method for Measuring Light Stability of Resilient Flooring by Color Change

This test method provides a means of measuring the amount of color change in flooring products when subjected to accelerated light exposure over a period of time (functional use of the flooring product).


ASTM F2657

Standard Test Method for Outdoor Weathering Exposure of Crosslinked Polyethylene (PEX) Tubing

This test method describes the procedure for exposing crosslinked polyethylene (PEX) tubing produced in accordance with Specification F 876 to natural (sunlight) ultraviolet (UV) radiation and evaluating the effects of the exposure.


ASTM G201

Standard Practice for Conducting Exposures in Outdoor Glass-Covered Exposure Apparatus with Air Circulation

This practice covers the basic principles and operating procedures for using outdoor glass-covered exposure apparatus with air circulation.


ASTM G24

Standard Practice for Conducting Exposures to Daylight Filtered Through Glass

This practice evaluates the resistance of nonmetallic materials to solar radiation filtered through glass.


ASTM G50

Standard Practice for Conducting Atmospheric Corrosion Tests on Metals

This practice covers and defines conditions for exposure of metals and alloys to the weather. It sets forth the general procedures that should be followed in any atmospheric test. It is presented as an aid in conducting atmospheric corrosion tests so that some of the pitfalls of such testing may be avoided. As such, it is concerned mainly with panel exposures to obtain data for comparison purposes.


ASTM G7

Standard Practice for Atmospheric Environmental Exposure Testing of Nonmetallic Materials

This practice covers procedures to be followed for direct exposure of nonmetallic materials to the environment. When originators of a weathering test have the actual exposure conducted by a separate agency, the specific conditions for the exposure of test and control specimens must be clearly defined and mutually agreed upon between all parties.


EN 12224 (DIN)

Geotextiles and Geotextile-Related Products - Determination of the Resistance to Weathering


EN 13523-19 (DIN)

Coil Coated Metals - Test Methods Part 19: Panel Design and Method of Atmospheric Exposure Testing


Ford DVM0020

Outdoor Weathering Tests

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


Ford FLTM BI 160-01

Florida and Arizona Outdoor Exposure Test


GM 2617M

Interior Trim Parts Performance

This specification covers the performance requirements of instrument panels, consoles, door trim, quarter trim panel, garnish moldings, armrests, headrests, assist handles, rear window trim panel and seat trims.


GM 3619M

Flexible Laminating Films and Film Plastic Laminates

This specification details the requirements for flexible plastic films that may be laminated to either metal or plastic substrates.


GM 7454M

Soft Interior Trim Parts

This standard covers the performance and approval requirements for three classes of soft interior trim parts.


GM 7455M

Decorative Interior Plastic Laminates and Films

This specification gives the durability requirements for plastic parts decorated with wood grains, or patterns for interior trim panels. The materials shall be classified into four types.


GM 9538P

Weathering Exposure Tests For Interior Trims

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


GMW 14873

Outdoor Weathering of Automotive Exterior Materials


GMW 3417

Natural Weathering Exposure Tests for Interior Trims/Materials

This test procedure describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.  The tests are conducted in climatic regions which offer extreme solar environments.


ISO 2810 (EN) (DIN)

Paints and Varnishes - Notes for Guidance on The Conduct of Natural Weathering Tests


ISO 4892-3 (EN) (DIN)

Plastics - Methods of Exposure to Laboratory Light Sources - Part 3: Fluorescent UV Lamps


ISO 877-1 (EN) (DIN)

Plastics - Methods of Exposure to Solar Radiation - Part 1: General Guidance


ISO 877-2 (EN) (DIN)

Plastics - Methods of Exposure to Solar Radiation - Part 2: Direct Weathering and Exposure Behind Window Glass


SAE J1976

Outdoor Weathering of Exterior Materials


SAE J2230

Accelerated Exposure of Automotive Interior Trim Material Using Outdoor Under-Glass Controlled Sun-Tracking Temperature and Humidity Apparatus

This SAE Standard specifies the operating procedure for the exposure of automotive interior trim materials in an outdoor behind-glass apparatus in which the temperature is controlled in a 24 h cycle.


Looking for a specific test standard? Search entire listing of all standards.

 

Recursos

Contate-nos

  1.  

Números de telefone Q-Lab

USA: +1-440-835-8700
Florida & Arizona Serviço de Teste: +1-305-245-5600
UK/Europe: +44-1204-861616
Alemanha: +49-681-857470
China: +86-21-5879-7970

 
View Full Site