ASTM D870

Standard Practice for Testing Water Resistance of Coatings Using Water Immersion

This practice covers the basic principles and operating procedures for testing water resistance of coatings by the partial or complete immersion of coated specimens in distilled or de-mineralized water at ambient or elevated temperatures.