ASTM D870

Standard Practice for Testing Water Resistance of Coatings Using Water Immersion

This practice covers the basic principles and operating procedures for testing water resistance of coatings by the partial or complete immersion of coated specimens in distilled or de-mineralized water at ambient or elevated temperatures.


ASTM D870

水浸法测试涂层耐水性的标准测试方法

本测试方法规定了涂层耐水性测试的基本原则和操作程序,通过在常温或高温下将涂层样品部分或完全浸泡在蒸馏水或软水中来进行测试。