Standards

佛罗里达户外曝晒测试标准

AAMA 2603

Voluntary Specification, Performance Requirements and Test Procedures For Pigmented Organic Coatings on Aluminum Extrusions and Panels

This specification describes test procedures and performance requirements for pigmented organic coatings applied to aluminum extrusions and panels.


AAMA 2603

铝合金型材和板材上的有机颜料涂层的推荐规格、性能要求和测试程序

本规范描述了用于铝合金型材和板材上的有机颜料涂层的测试程序和性能要求。


AAMA 2605

Voluntary Specification, Performance Requirements and Test Procedures for Superior Performing Organic Coatings on Aluminum Extrusions and Panels

This specification describes test procedures and performance requirements for superior performing organic coatings applied to aluminum extrusions and panels for architectural products.


AAMA 2605

铝合金型材和板材上的超级性能有机涂料的推荐规格、性能要求和测试程序

本规范描述了超级性能有机涂料的测试程序和性能要求,这类涂料适用于建筑产品(铝合金型材和板材)。


AATCC TM111

Weather Resistance of Textiles: Exposure to Daylight and Weather

This test method provides a means for determining the weather resistance of textile materials.


AATCC TM111

纺织品的耐候性 暴露于日光和气候

本测试方法提供了测定纺织材料耐候性的途径。


ASTM C1589

Standard Practice for Outdoor Weathering of Construction Seals and Sealants

This practice describes outdoor exposure procedures used to determine the weathering durability of building construction, seals and sealants.


ASTM C1589

建筑密封件和密封剂户外老化的标准测试方法

本测试方法描述了用于测定建筑结构密封件和密封剂老化耐候性的户外曝露测试程序。


ASTM D1006

Standard Practice for Conducting Exterior Exposure Tests of Paints on Wood

This practice covers procedures to be followed for direct exposure of house and trim paints on new, previously unpainted wood materials to the environment.


ASTM D1006

木器涂料外观曝露测试的标准测试方法

本测试方法规定了对房屋和新的、以前未上漆的木质材料上的装饰涂料直接曝露在环境中要遵循的程序。


ASTM D1014

Standard Practice for Conducting Exterior Exposure Tests of Paints and Coatings on Metal Substrates

This practice covers procedures to be followed for direct exposure of exterior paints and coatings to the environment when applied to metal surfaces.


ASTM D1014

金属底板上油漆和涂料外观曝露测试的标准测试方法

本测试方法规定了对用于金属表面的外部油漆和涂料直接曝露在环境中要遵循的程序。


ASTM D1435

Standard Practice for Outdoor Weathering of Plastics

This practice is intended to cover procedures for the exposure of plastic materials to weather. Note 1See Practice G 24 for aging under glass.


ASTM D1435

塑料户外老化标准测试方法

本测试方法旨在规定塑料材料进行曝露老化测试的程序。 请参见测试方法 G 24 玻璃下老化现象。


ASTM D1670

Standard Test Method for Failure End Point in Accelerated and Outdoor Weathering of Bituminous Materials

This test method covers the use of a spark generating apparatus for determination of failure due to cracking of bituminous materials undergoing accelerated or outdoor weathering on electrically conductive backings.


ASTM D1670

沥青材料加速和户外老化失效终点的标准测试方法

该测试方法规定了使用火花发生装置测定在导电底材上经加速或户外老化沥青材料的开裂失效。


ASTM D3424

Standard Practice for Evaluating the Relative Lightfastness and Weatherability of Printed Matter

This standard describes procedures for the determination of the relative lightfastness and weatherability of printed matter under the following conditions, which involve exposure to natural daylight or accelerated procedures in the laboratory.


ASTM D3424

印刷品相对日晒色牢度和耐候性评估的标准测试方法

这个标准描述了印刷品在下列情况下相对日晒色牢度和耐候性的评估程序,涉及自然光曝露测试程序或实验室加速曝露测试程序。


ASTM D3456

Standard Practice for Determining by Exterior Exposure Tests the Susceptibility of Paint Films to Microbiological Attack

This practice provides guidelines for determining the susceptibility of paint films to microbiological attack on exterior exposure. While it is recognized that various organisms may occur on an exposed coating, the specific types of organisms are mainly of academic interest. The degree to which microbiological discoloration occurs is the primary concern.


ASTM D3456

漆膜对微生物攻击的敏感性的外部曝露测定的标准测试方法

本指南对测定曝露在外部的漆膜受微生物攻击的影响提供指导。 虽然人们认识到,曝露的涂层上可能会出现各种生物体,但研究的重点主要集中在特定类型的生物体上。 在微生物变色的程度是首要关注的问题。


ASTM D3679

Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Siding

This specification establishes requirements and test methods for the materials, dimensions, warp, shrinkage, impact strength, expansion, appearance, and windload resistance of extruded single-wall siding manufactured from rigid (unplasticized) PVC compound. Methods of indicating compliance with this specification are also provided.


ASTM D3679

硬性聚氯乙烯(PVC)墙板标准规范

本规范规定了对挤压单壁壁板的要求和测试方法,包括材料、尺寸、翘曲、收缩、冲击强度、膨胀、外观和风阻,壁板由刚性(未增塑)PVC复合物制造而成。 还提供了表明符合本规范的方法。


ASTM D4101

Standard Specification for Polypropylene Injection and Extrusion Materials

This specification covers polypropylene materials suitable for injection molding and extrusion. Polymers consist of homopolymer, copolymers, and elastomer compounded with or without the addition of impact modifiers (ethylene-propylene rubber, polyisobutylene rubber, and butyl rubber), colorants, stabilizers, lubricants, or reinforcements.


ASTM D4101

聚丙烯注塑和挤出材料的标准规范

本规范规定了聚丙烯材料的注塑成型和挤出。 聚合物包括均聚物、共聚物及复合弹性体(加或不加聚异丁烯橡胶、乙丙橡胶、丁基橡胶等冲击改性剂),还有色素、稳定剂、润滑剂或增强剂。


ASTM D4303

Standard Test Methods for Lightfastness of Colorants Used in Artists' Materials

Four test methods to accelerate the effects of long term indoor illumination on artists' materials are described.


ASTM D4303

艺术材料中使用的着色剂光稳定性的标准测试方法

描述了4种加速长期室内照明对艺术材料的影响的测试方法。


ASTM D4726

Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Exterior-Profile Extrusions Used for Assembled Windows and Doors

This specification establishes requirements for the material properties, including dimensional stability, weatherability, and extrusion quality, of rigid poly(vinyl chloride) (PVC) exterior profile extrusions used for assembled windows and doors.


ASTM D4726

用于组装门窗的刚性聚氯乙烯(PVC)外部轮廓型材的标准规范

本规范规定了对材料特性的要求,包括尺寸稳定性、耐候性和挤出质量,材料是组装门窗用刚性聚氯乙烯(PVC)外部轮廓型材。


ASTM D5272

Standard Practice for Outdoor Exposure Testing of Photodegradable Plastics

This practice defines test conditions applicable when Practices D1435 and G7 are employed for the outdoor exposure testing of photodegradable plastics.


ASTM D5272

光降解塑料户外曝露测试的标准测试方法

本测试方法规定了按D1435和G7测试法方法对塑料进行光降解户外曝露测试时可用的测试条件。


ASTM D5819

Standard Guide for Selecting Test Methods for Experimental Evaluation of Geosynthetic Durability

This guide covers a designer/specifier through a systematic determination of those factors of the appropriate application environment that may affect the post-construction service life of a geosynthetic.


ASTM D5819

土工合成材料耐候性测试评估方法选择的标准指南

本指南系统地设计/明确了可能影响土工合成材料施工后的使用寿命的环境因素。


ASTM D5970

Standard Test Method for Deterioration of Geotextiles from Outdoor Exposure

This test method covers evaluating the deterioration in tensile strength and strain after outdoor exposure.


ASTM D5970

土工布户外曝晒老化的标准测试方法

该测试方法规定了户外曝露后的拉伸强度和应变退化的评估。


ASTM D6551

Standard Practice for Accelerated Weathering of Pressure-Sensitive Tapes by Xenon-Arc Exposure Apparatus

This practice describes one environment for the exposure of pressure-sensitive tape, used primarily for packaging, to a laboratory accelerated weathering environment.


ASTM D6551

使用氙灯曝露装置对与压力敏感的带材进行加速老化的标准测试方法

本测试方法描述了实验室加速老化环境下对与压力敏感的带材进行曝露测试,主要用于包装材料。


ASTM D6662

Standard Specification for Polyolefin-Based Plastic Lumber Decking Boards

This specification covers polyolefin-based plastic lumber products for use as exterior residential decking boards.


ASTM D6662

聚烯烃基木塑装饰板的标准规范

本规范规定了住宅外墙板用聚烯烃塑料板材的使用。


ASTM D6864

Standard Specification for Color and Appearance Retention of Solid Colored Plastic Siding Products

This specification establishes requirements and test methods for the color and appearance retention of solid colored plastic siding products.


ASTM D6864

固体彩色塑料壁板产品颜色和外观保持的标准规范

本规范规定了对固体彩色塑料壁板产品颜色和外观保持的要求和测试方法。


ASTM D7251

Standard Specification for Color and Appearance Retention of Variegated Color Plastic Siding Products

This specification establishes requirements and test methods for the color and appearance retention of variegated color plastic siding products.


ASTM D7251

杂色塑料壁板产品颜色和外观保持的标准规范

本规范规定了对杂色塑料壁板产品颜色和外观保持的要求和测试方法。


ASTM D7869

Standard Practice for Xenon Arc Exposure Test with Enhanced Light and Water Exposure for Transportation Coatings

This test procedure is used to simulate the physical and environmental stresses that a coating for exterior transportation applications (for example, automotive) is exposed to in a subtropical climate, such as southern Florida.


ASTM E782

Standard Practice for Exposure of Cover Materials for Solar Collectors to Natural Weathering Under Conditions Simulating Operational Mode

This practice provides a procedure for the exposure of cover materials for flat-plate solar collectors to the natural weather environment at temperatures that are elevated to approximate operating conditions.


ASTM E782

太阳能聚集器覆盖材料在模拟运行模式条件下自然老化曝露测试的标准测试方法

本测试方法提供了平板型太阳能集热器覆盖材料在自然气候环境下(温度升高至近似运行状况)的曝露测试程序。


ASTM E881

Standard Practice for Exposure of Solar Collector Cover Materials to Natural Weathering Under Conditions Simulating Stagnation Mode

This practice covers a procedure for the exposure of solar collector cover materials to the natural weather environment at elevated temperatures that approximate stagnation conditions in solar collectors having a combined back and edge loss coefficient of less than 1.5 W/(m2 · °C).


ASTM E881

太阳能聚集器覆盖材料在模拟停滞模式条件下自然老化曝露测试的标准测试方法

本测试方法规定了太阳能集热器覆盖材料在高温自然气候环境下的曝露测试程序,太阳能集热器一直保持在高温状态,其背面和边缘损失系数小于1.5瓦/M2.0C。


ASTM F1164

Standard Test Method for Evaluation of Transparent Plastics Exposed to Accelerated Weathering Combined with Biaxial Stress

This test method covers the resistance of transparent plastics exposed to environmental conditioning (accelerated weathering) under a biaxial stress state induced by a pressure cell/test fixture.


ASTM F1164

透明塑料受到双轴应力与加速老化暴露评估的标准测试方法

本测试方法规定了透明塑料在压力部件/测试支架导致的双轴应力状态下曝露于环境条件(加速老化)的抵抗力。


ASTM F1515

Standard Test Method for Measuring Light Stability of Resilient Flooring by Color Change

This test method provides a means of measuring the amount of color change in flooring products when subjected to accelerated light exposure over a period of time (functional use of the flooring product).


ASTM F2657

Standard Test Method for Outdoor Weathering Exposure of Crosslinked Polyethylene (PEX) Tubing

This test method describes the procedure for exposing crosslinked polyethylene (PEX) tubing produced in accordance with Specification F 876 to natural (sunlight) ultraviolet (UV) radiation and evaluating the effects of the exposure.


ASTM F2657

交联聚乙烯(PEX)管户外老化曝露测试的标准测试方法

本测试方法描述了按F 876规范生产的交联聚乙烯(PEX)管在自然(阳光)紫外线(UV)辐射下的曝露测试程序和暴露效果评估程序。


ASTM G201

Standard Practice for Conducting Exposures in Outdoor Glass-Covered Exposure Apparatus with Air Circulation

This practice covers the basic principles and operating procedures for using outdoor glass-covered exposure apparatus with air circulation.


ASTM G201

在有空气流通的户外玻璃框装置下进行曝露测试的标准测试方法

本测试方法是关于有空气流通的户外玻璃框曝露装置的基本原则和操作程序。


ASTM G24

Standard Practice for Conducting Exposures to Daylight Filtered Through Glass

This practice evaluates the resistance of nonmetallic materials to solar radiation filtered through glass.


ASTM G24

在透过玻璃的日光下进行曝露试验的标准测试方法

本测试方法评估非金属材料对透过玻璃的太阳辐射的抵抗力。


ASTM G50

Standard Practice for Conducting Atmospheric Corrosion Tests on Metals

This practice covers and defines conditions for exposure of metals and alloys to the weather. It sets forth the general procedures that should be followed in any atmospheric test. It is presented as an aid in conducting atmospheric corrosion tests so that some of the pitfalls of such testing may be avoided. As such, it is concerned mainly with panel exposures to obtain data for comparison purposes.


ASTM G50

金属大气腐蚀试验的标准测试方法

本测试方法包括并定义了金属和合金曝露测试的气候条件。 说明了任何大气测试应遵循的一般程序。 可帮助避免大气腐蚀测试中的一些缺陷。 因此,对比测试时主要考虑从曝晒面板获取的数据。


ASTM G7

Standard Practice for Atmospheric Environmental Exposure Testing of Nonmetallic Materials

This practice covers procedures to be followed for direct exposure of nonmetallic materials to the environment. When originators of a weathering test have the actual exposure conducted by a separate agency, the specific conditions for the exposure of test and control specimens must be clearly defined and mutually agreed upon between all parties.


ASTM G7

非金属材料大气环境曝露试验的标准测试方法

本测试方法是非金属材料直接曝露在环境中的操作程序。当老化测试客户委托独立的机构进行实际曝露测试时,暴露测试和样品制备的具体情况必须明确界定,且试验各方之间必须达成共识。


EN 12224 (DIN)

Geotextiles and Geotextile-Related Products - Determination of the Resistance to Weathering


EN 13523-19 (DIN)

Coil Coated Metals - Test Methods Part 19: Panel Design and Method of Atmospheric Exposure Testing


Ford DVM0020

Outdoor Weathering Tests

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


Ford FLTM BI 160-01

Florida and Arizona Outdoor Exposure Test


Ford FLTM BI 160-01

佛罗里达和亚利桑那的户外曝露测试


GM 2617M

Interior Trim Parts Performance

This specification covers the performance requirements of instrument panels, consoles, door trim, quarter trim panel, garnish moldings, armrests, headrests, assist handles, rear window trim panel and seat trims.


GM 3619M

Flexible Laminating Films and Film Plastic Laminates

This specification details the requirements for flexible plastic films that may be laminated to either metal or plastic substrates.


GM 7454M

Soft Interior Trim Parts

This standard covers the performance and approval requirements for three classes of soft interior trim parts.


GM 7455M

Decorative Interior Plastic Laminates and Films

This specification gives the durability requirements for plastic parts decorated with wood grains, or patterns for interior trim panels. The materials shall be classified into four types.


GM 9538P

Weathering Exposure Tests For Interior Trims

This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.


GMW 14873

Outdoor Weathering of Automotive Exterior Materials


GMW 14873

汽车外饰材料户外老化


GMW 3417

Natural Weathering Exposure Tests for Interior Trims/Materials

This test procedure describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.  The tests are conducted in climatic regions which offer extreme solar environments.


ISO 2810 (EN) (DIN)

Paints and Varnishes - Notes for Guidance on The Conduct of Natural Weathering Tests


ISO 2810 (EN) (DIN)

色漆和清漆 - 自然老化测试实施的指导注意事项


ISO 4892-3 (EN) (DIN)

Plastics - Methods of Exposure to Laboratory Light Sources - Part 3: Fluorescent UV Lamps


ISO 4892-3 (EN) (DIN)

塑料–使用实验室光源进行曝露测试的方法–第三部分 荧光紫外灯


ISO 877-1 (EN) (DIN)

Plastics - Methods of Exposure to Solar Radiation - Part 1: General Guidance


ISO 877-1 (EN) (DIN)

塑料–太阳辐射曝露方法–第一部分 一般指导


ISO 877-2 (EN) (DIN)

Plastics - Methods of Exposure to Solar Radiation - Part 2: Direct Weathering and Exposure Behind Window Glass


ISO 877-2 (EN) (DIN)

塑料–太阳辐射曝露方法–第二部分 直接暴露和玻璃框下暴露


SAE J1976

Outdoor Weathering of Exterior Materials


SAE J1976

外部材料户外老化


SAE J2230

Accelerated Exposure of Automotive Interior Trim Material Using Outdoor Under-Glass Controlled Sun-Tracking Temperature and Humidity Apparatus

This SAE Standard specifies the operating procedure for the exposure of automotive interior trim materials in an outdoor behind-glass apparatus in which the temperature is controlled in a 24 h cycle.


SAE J2230

使用户外玻璃下控制阳光跟踪温度和湿度的设备对汽车内饰材料进行加速曝露测试

本SAE标准规定了汽车内饰材料曝露测试的操作程序,使用户外玻璃下装置,其温度每天24小时可控。


Looking for a specific test standard? Search entire listing of all standards.

 

资源

联系我们

  1.  

Q-Lab 电话号码

美国:+1-440-835-8700
佛罗里达及亚利桑那企业管理:+1-305-245-5600
英国/欧洲:+44-1204-861616
德国:+49-681-857470
中国:+86-21-5879-7970

 
View Full Site