Q-TRAC 自然太阳光 聚能装置测试标准

AAMA 624

Voluntary Specification, Performance Requirements and Test Procedures for High Performance Organic Coatings on Fiber Reinforced Thermoset Profiles

This specification describes test procedures and performance requirements for high performance, organic, coatings applied to fiber reinforced thermoset profiles for windows, doors and similar products.


AAMA 624

纤维增强热固性型材上的高性能有机涂层的推荐规格、性能要求和测试程序

本规范描述了高性能有机涂料的测试程序和性能要求,这类涂料应用于纤维增强热固性型材(窗、门和类似的产品)。


ASTM D4141

Standard Practice for Conducting Black Box and Solar Concentrating Exposures of Coatings

This practice covers two accelerated outdoor exposure procedures for evaluating the exterior durability of coatings applied to substrates.


ASTM D4141

涂层的黑箱和太阳光聚能装置试验的标准测试方法

本测试方法规定了两个户外加速曝露测试程序,用于底板涂料户外耐候性评估。


ASTM D4364

Standard Practice for Performing Outdoor Accelerated Weathering Tests of Plastics Using Concentrated Sunlight

This practice covers the use of Fresnel-reflecting concentrators that use the sun as a source of ultraviolet (UV) and longer wavelength radiation. Such devices are used in the outdoor accelerated exposure testing of plastics.


ASTM D4364

使用太阳光聚能装置对塑料进行户外加速老化的标准测试方法

本测试方法规定了菲涅尔反射聚光器(用太阳作为紫外线(UV)辐射源和长波辐射源)的使用。 该装置用于塑料户外加速曝露测试。


ASTM D5105

Standard Practice for Performing Accelerated Outdoor Weathering of Pressure-Sensitive Tapes Using Concentrated Natural Sunlight

This practice covers one procedure for the exposure of pressure-sensitive tapes to an accelerated outdoor weathering environment.


ASTM D5105

使用太阳光聚能装置对与压力敏感的带材进行户外加速老化的标准测试方法

本测试方法规定了户外加速老化环境下对与压力敏感的带材的曝露测试的程序。


ASTM G90

Standard Practice for Performing Accelerated Outdoor Weathering of Nonmetallic Materials Using Concentrated Natural Sunlight

Fresnel-reflecting concentrators using the sun as source are utilized in the accelerated outdoor exposure testing of nonmetallic materials.


ASTM G90

使用太阳光聚能装置对非金属材料进行户外加速老化试验的标准测试方法

菲涅尔反射聚集器用太阳作为光源,用于非金属材料户外加速曝露测试。


ISO 877-3 (EN) (DIN)

Plastics - Methods of Exposure to Solar Radiation - Part 3: Intensified Weathering Using Concentrated Solar Radiation


ISO 877-3 (EN) (DIN)

塑料–太阳辐射曝露方法–第三部分 用聚集的太阳辐射的增强老化


SAE J1961

Accelerated Exposure of Automotive Exterior Materials Using a Solar Fresnel Reflector Apparatus


SAE J1961

使用太阳光菲涅尔反射装置对汽车外饰材料进行加速曝露测试


该测试方法指定了使用太阳光菲涅尔反射装置对各种汽车材料进行加速曝露测试的操作程序。


SAE J576

Plastic Material or Materials for Use in Optical Parts Such as Lenses and Reflex Reflector of Motor Vehicle Lighting Devices

This SAE Recommended Practice provides test methods and requirements to evaluate the suitability of plastic material or materials intended for optical application in motor vehicles.


SAE J576

塑料材料或用于光学零件如机动车辆照明设备的透射镜和反射镜的材料

本SAE标准提供了评估塑料材料或汽车光学应用材料稳定性的测试方法和要求。


Looking for a specific test standard? Search entire listing of all standards.

 

资源

联系我们

  1.  

Q-Lab 电话号码

美国:+1-440-835-8700
佛罗里达及亚利桑那企业管理:+1-305-245-5600
英国/欧洲:+44-1204-861616
德国:+49-681-857470
中国:+86-21-5879-7970

 
View Full Site