US Webinar - How to Run SAE J2334

Join the technical experts at Q-Lab for a live session on How to Run SAE J2334. We will present at 8 am and 11 am EDT on Thursday, 30 April. 


Q-Lab's technical applications team is presenting a two-part series this spring focusing on how to perform and understand some important international automotive corrosion testing standards. The second installment in this series focuses on SAE J2334: Laboratory Cyclic Corrosion Test.

SAE J2334 is a widely-used protocol for conducting accelerated laboratory corrosion testing of automotive paints and other components. This standard includes some requirements that may be challenging for some users to interpret and execute properly. In this new presentation, Q-Lab experts will explain and provide recommendations for the important features of this test, including:

  • Electrolyte solution preparation
  • High humidity requirements
  • Salt application
  • Test monitoring using corrosion coupons

A case study is included that illustrates how controlling transitions between wet and dry steps can help improve test-to-test repeatability, and how the use of mass-loss corrosion coupons can help verify consistent chamber performance.

Join us for this new webinar content! If you're interested in the first part of this series, be sure to check out Corrosion Accelerated Test with Controlled Humidity (CATCH), a new test protocol specifically designed for aluminum automotive components.

This webinar will be presented in English.