LX-5029 Accelerated Acid Etch Part II
Technical Bulletins
LX-5029
Download FileAbstract For decades, automotive coatings have experienced degradation in the form of etching on coatings exposed to acid rain. As a result, procedures were developed to simulate and accelerate this type of degradation. These proced...