Color is an important performance characteristic for many plastic products exposed to outdoor environments. Sunlight, heat, and moisture can affect both the polymer and its pigments, resulting in fading, yellowing, darkening, and other changes in appearance.
In Q-Lab’s recent webinar, Color Change in Weathering Testing of PVC Plastics, our technical experts examined how different weathering exposures affect colored PVC materials. The webinar compared natural outdoor exposure with several accelerated laboratory methods and explored what the results reveal about selecting and validating an accelerated weathering test.
Understanding Weathering of Plastics
Weathering results from the combined effects of sunlight, heat, and water. For plastics, these environmental stresses can affect the base polymer, pigments, or both, making it important to understand not only how much a material changes, but also why that change occurs.
The webinar focused on color change in PVC plastics, particularly as organic color additives increasingly replace inorganic additives. While organic pigments can offer advantages, they may also have lower lightfastness. Different wavelengths of sunlight can also produce different effects, including yellowing and color fade.
Comparing Outdoor and Accelerated Weathering
A key theme of the webinar was the importance of using both natural outdoor and accelerated laboratory testing.
For the study presented, nine colored PVC materials were exposed outdoors in Florida and tested using several accelerated methods. Laboratory exposures included xenon arc testing with different optical filters and fluorescent UV testing with UVA-340 and UVB-313 lamps.
These different light sources do not produce identical spectral power distributions. The wavelengths to which a material is exposed can have a significant effect on the type of degradation that occurs.
What Can Color Change Tell Us?
Color change was measured using Delta E (ΔE), which provides a numerical measurement of total color change based on changes in lightness and color coordinates.
However, the study demonstrated why Delta E alone does not always tell the complete story. Some specimens experienced darkening associated with PVC polymer degradation, while others experienced fading associated with pigment degradation. The red and pink specimens provided particularly clear examples of how different exposure spectra can produce different modes of color change.
This distinction is important because two tests can produce significant color change without necessarily reproducing the same degradation mechanism.
Correlating Accelerated Testing with Outdoor Results
When the accelerated test results were compared with Florida outdoor exposure, xenon arc testing with Daylight and Extended UV filters and fluorescent UV testing with UVA-340 lamps demonstrated strong rank-order correlation for color change. UVB-313 produced substantially poorer correlation in this particular study.
The results highlight an important principle in weathering testing: there is no universal acceleration factor or test condition that works for every material. Weathering behavior is material-dependent, and a test that correlates well for color change may not necessarily correlate well for other physical properties. Outdoor weathering data therefore remains important for validating accelerated laboratory methods.
Key Takeaways
- Sunlight, heat, and water are the primary forces responsible for weathering.
- Different wavelengths of light can produce different degradation mechanisms in plastics.
- Total color change is useful, but understanding the type of color change is also important.
- Accelerated testing should be correlated with natural outdoor weathering to confirm that it produces meaningful results.
- Weathering performance is material-dependent, and changes in material chemistry may require retesting.
- A combination of outdoor and accelerated laboratory testing can provide a more complete understanding of material durability.
Learn More About Weathering Testing of Plastics
Understanding how and why plastics change during weathering can help manufacturers select more appropriate test methods and make better-informed decisions about material durability.
Watch the full webinar to explore the PVC test program and results in greater detail, including comparisons between Florida outdoor exposure, xenon arc testing, and fluorescent UV testing. We also have an extensive webinar library on-demand covering a wide variety of weathering and corrosion topics. You can access them anytime at Q-Lab.com/webinars.
You can also learn more about Q-Lab’s Q-SUN xenon arc weathering testers, QUV accelerated weathering testers, and natural outdoor weathering testing services to explore options for evaluating the weathering performance of plastics.
Frequently Asked Questions
Q: Why should outdoor and accelerated weathering testing be used together?
A: Outdoor testing provides real-world weathering data that can be used to validate accelerated laboratory methods. Accelerated testing can then provide results in a shorter timeframe while maintaining confidence that the test is producing relevant degradation.
Q: Does a higher Delta E always mean a material performed worse?
A: Not necessarily. Delta E measures the magnitude of total color change, but it does not identify the mechanism responsible for that change. The webinar demonstrated that polymer degradation and pigment degradation can produce different types of color change, making additional characterization important.
Q: Why does the light source matter when testing colored plastics?
A: Different wavelengths can affect the polymer and pigments differently. In the study, shortwave UV contributed to plastic yellowing, while visible light contributed to pigment fading. The spectrum used in an accelerated test can therefore influence both the amount and type of degradation observed.
Q: Can one accelerated weathering test be used for every plastic?
A: No single accelerated test or acceleration factor applies to every material. Weathering is strongly material-dependent, and changes to a material's chemistry can change its response to weathering. Accelerated methods should be validated against appropriate outdoor data.