Webinar Recap: Lightfastness Testing of Textiles


Color is an important performance characteristic for textiles used in apparel, automotive interiors, furnishings, and outdoor applications. Over time, exposure to light can cause fading and other changes that affect a textile’s appearance and performance.

In Q-Lab’s recent webinar, Lightfastness Testing of Textiles, our technical experts discussed how light affects textile materials, how lightfastness is evaluated, and how common test standards are used to assess resistance to color change.

What Is Textile Lightfastness?

Lightfastness describes a textile’s ability to resist color change caused by exposure to light, primarily sunlight. These changes result from photochemical processes involving ultraviolet and visible radiation and can also be influenced by temperature and humidity. The lightfastness of a textile can vary considerably depending on the dye or colorant used. 

The webinar also explained the distinction between lightfastness and weathering. Lightfastness testing focuses primarily on the effects of sunlight and color degradation, while weathering considers additional environmental factors such as heat and water and may evaluate longer-term fading and fiber degradation. 

How Is Lightfastness Evaluated?

Standard reference materials play an important role in textile lightfastness testing. Blue Wool references, for example, provide known levels of lightfastness that can be used to help determine exposure duration, verify test conditions, and compare the performance of test specimens. 

After exposure, color change can be evaluated using methods such as Blue Wool references, Grey Scales, or instrumental color measurement. Each provides a different way to assess how a textile has changed during testing. 

Accelerated Lightfastness Testing

Accelerated lightfastness testing can be performed using Q-SUN xenon arc weathering testers. Xenon arc light sources reproduce full-spectrum sunlight, while optical filters can be used to simulate specific exposure environments, such as sunlight through window glass.

Our webinar explored two major textile lightfastness standards, ISO 105-B02 and AATCC TM16.3. Although both use xenon arc exposure, their test conditions differ in areas such as temperature, humidity, and optical filtration. 

Other standards within the ISO 105-B series address different applications and environments, including outdoor textiles and higher-temperature exposures. Selecting the appropriate method depends on the textile’s intended use and the conditions it is expected to experience. 

Key Takeaways
  • Lightfastness measures a textile’s resistance to color change from exposure to light.
  • Dye chemistry, temperature, and humidity can influence lightfastness performance.
  • Reference materials such as Blue Wool are commonly used to help control and evaluate textile lightfastness tests.
  • Xenon arc testing provides an accelerated method for evaluating textile lightfastness.
  • ISO 105-B02 and AATCC TM16.3 are two important textile lightfastness standards, but their exposure conditions are not identical.
  • The appropriate test method depends on the textile and its intended service environment. 
     
Learn More About Textile Lightfastness Testing

Want to take a deeper look at textile lightfastness testing? Watch the full webinar to learn more about reference materials, evaluation methods, xenon arc testing, ISO 105-B02, AATCC TM16.3, and other considerations for developing an effective textile testing program. We also have an extensive webinar library on-demand covering a wide variety of weathering and corrosion topics. You can access them anytime at Q-Lab.com/webinars. 

You can also learn more about Q-SUN xenon arc weathering testers or explore Q-Lab’s weathering resources for additional information on weathering and lightfastness testing. Need more technical help? Our team of experts is available. Just contact us here and we will get in touch with you directly! 


Frequently Asked Questions

Q: Why are Blue Wool references used in textile lightfastness testing?

A: Blue Wool materials have known lightfastness characteristics and can be used to establish exposure duration, verify test conditions, and compare fading of test specimens.

Q: What is the difference between lightfastness and weathering?

A: Lightfastness primarily focuses on color change caused by light exposure. Weathering considers a broader combination of environmental stresses, including sunlight, heat, and water.

Q: Are ISO 105-B02 and AATCC TM16.3 the same test?

A: No. Both use xenon arc exposure, but their specified conditions differ, including temperature, relative humidity, and optical filtration. 

Q: How do I choose the appropriate textile testing standard?

A: Test selection should reflect the textile’s intended application and exposure environment. Apparel, automotive textiles, and outdoor textiles may require different test methods and exposure conditions.