Webinar Recap: Why Test in Arizona? Understanding Weathering in Dry Climates


When testing materials for outdoor use, the climate where testing takes place is important. Materials can age differently in wet and dry climates, which means the location selected for outdoor exposure testing can affect the results.

Florida is a primary benchmark for weathering in moderate and wet climates. Arizona serves as the benchmark for dry climates. As Q-Lab’s Mike Crewdson explained during this webinar, a Florida test will not provide accurate results for a product intended for a dry climate, just as an Arizona test will not provide accurate results for a product intended for a wet climate.

How Climate Affects Material Degradation

Three factors play an important role in weathering:

  • Solar radiation: Solar radiation, especially UV, provides the energy needed to break bonds in the chemical structure of a material.
  • Temperature: Heat and thermal cycling can affect the rate of chemical reactions.
  • Moisture: Water as condensation, rain, and humidity can change the type of failure that occurs.

This is why exposure in different climates can produce different results.

In wet climates, plastics can experience biological growth, chalking, ductile failures, warping, color changes, and checking. In dry climates, materials can experience yellowing, browning, brittle failures, cracking, and crumbling.

The difference in failure modes is important when evaluating a material. If testing produces a different failure from the one that occurs in actual use, the resulting conclusion may be incorrect.

Florida and Arizona: What Is Different?

This webinar compared Miami, Florida, with Phoenix, Arizona. The average temperature in both locations is about 30 °C (86 °F). UV exposure is only slightly higher in Arizona, while the average temperature is the same. Arizona does have higher temperature highs and lower temperature lows. However, the water content is very different between the two locations.

ParameterMiami, FloridaPhoenix, Arizona
Total solar energy6,500 MJ/m²8,200 MJ/m²
UV energy320 MJ/m²360 MJ/m²
Average temperature30 °C30 °C
Annual rainfall1,600 mm250 mm
Average relative humidity80%30%
Annual wet time4,500 hours200 hours

During summer, the differences become even more pronounced. Phoenix can reach an air temperature of 45 °C and a black panel temperature of 65 °C, compared with 32 °C and 55 °C in Miami. Relative humidity can range from 5% to 20% in Phoenix, compared with 70% to 100% in Miami.

Dry ClimateWhy Dry Climate Testing Matters

Dry climates are important because many products are used in regions where humidity and rainfall are low. Product types affected by dry climates include:

  • Roofing materials
  • Shingles and underlay
  • Windows and doors
  • Siding
  • Gutters
  • Outdoor furniture
  • Automotive trim

Dry climates are also found in many parts of the world, including the western United States, North Africa, the Middle East, the Arabian Peninsula, Central Asia, South Africa, interior Australia, and western South America. For products intended for these areas, testing in a dry benchmark climate can provide data that represents the conditions where the product will be used.

Q-Lab ArizonaWhy Arizona? 

Central Arizona has been a benchmark for dry climate testing since 1950 due to its high temperatures, high solar radiation and a high percentage of direct beam energy. Clear skies support high UV levels and long periods of effective UV exposure. Arizona is also very dry year-round.

Importantly compared to other hot, arid regions of the world, Arizona is accessible and developed, meaning that the infrastructure to conduct exposure testing and perform evaluations is readily available.

Arizona may appear extreme, but the presentation notes that its conditions are not unrealistic. Summer conditions in other locations can approach the temperatures found in Arizona. For products intended for dry climates, this can provide faster results while maintaining exposure to an outdoor environment.
 

Key Takeaways
  • Materials can age differently in wet and dry climates.
  • Moisture is a major difference between Florida and Arizona.
  • Arizona is a benchmark location for dry climate testing.
  • Products intended for dry regions should be tested in a climate that represents their intended use.
  • Arizona combines sunlight, UV, temperature, and dryness to provide an accelerated test for dry climate applications.
     

Frequently Asked Questions

Q: Why can't Florida be used for every product?

A: Florida represents a wet climate, while Arizona represents a dry climate. Since moisture can change the type of failure that occurs, testing in Florida may not produce the same failure as testing in a dry climate.

Q: What is the biggest difference between Florida and Arizona?

A: The presentation identifies water content as the major difference. Arizona has much less rainfall, lower humidity, and less wet time than Florida.

Q: What types of products can be affected by dry climates?

A: Roofing materials, plastic building products, outdoor furniture, and automotive trim are all excellent examples.

Q: Why is Arizona considered a benchmark for dry climate testing?

A: Central Arizona provides high solar radiation, high temperatures, very low humidity, and limited rainfall. It has been a benchmark for dry climate testing since 1950.

Learn More About Outdoor Weathering Testing

Want to learn more about choosing the right outdoor exposure location for your materials?

Explore Q-Lab's outdoor weathering testing services to learn more about testing in Florida and Arizona.

Learn more about Q-Lab's natural outdoor testing locations and how exposure conditions can affect material performance.

Have questions about your testing program? Contact Q-Lab to discuss your material and testing needs.

The first part of this webinar series focused on natural outdoor weathering testing in Florida. You can download the slides or watch the recording here.