Standards

Q-SUN 氙灯试验箱测试标准

AATCC TM16

Colorfastness to Light

This test method provides the general principles and procedures which are currently in use for determining the colorfastness to light of textile materials.


AATCC TM16

耐光色牢度

本测试方法提供了目前用来测定纺织材料日晒色牢度的一般原则和程序。


AATCC TM169

Weather Resistance of Textiles: Xenon Lamp Exposure

This test method provides the procedure for the exposure of textile materials of all kinds, including coated fabrics and products made thereof, in an artificial weathering apparatus using controlled conditions of test.


AATCC TM169

纺织品的耐候性 氙灯曝露测试

本测试方法提供了各类纺织品材料(包括涂层织物和由其制造的产品)在受控测试条件下用人工老化仪器进行曝露测试的测试程序。


ASTM C1257

Standard Test Method for Accelerated Weathering of Solvent-Release-Type Sealants

This test method includes two laboratory accelerated exposure procedures for predicting the effects of ultraviolet or ultraviolet/visible radiation, heat, and moisture on color, chalking, cracking, and adhesion of solvent-release sealants.


ASTM C1257

溶剂释放型密封剂加速老化的标准测试方法

该测试方法包括两个实验室加速暴露测试程序,用于预测紫外线或紫外线/可见光辐射、热量和湿气对溶剂释放型密封剂的颜色、粉化、开裂和附着力的影响。


ASTM C1442

Practice for Conducting Tests on Sealants Using Artificial Weathering Apparatus

This practice covers three types of laboratory weathering exposure procedures for evaluating the effect of actinic radiation, heat, and moisture on sealants.


ASTM C1442

使用人工老化设备对密封剂进行测试的方法

本测试方法包括三种实验室加速老化曝露程序,评估太阳光辐射、热和潮湿对密封剂的影响。


ASTM C1519

Standard Test Method for Evaluating Durability of Building Construction Sealants by Laboratory Accelerated Weathering Procedures

This test method covers the method for the determination of the durability of a sealant based on its ability to function in cyclic movement maintaining adhesion and cohesion after repeated exposure to laboratory accelerated weathering procedures.


ASTM C1519

实验室加速老化对建筑结构密封剂耐候性评估的标准测试方法

该测试方法是密封剂耐候性的测定方法,是基于在依据实验室加速老化程序反复曝露后,密封剂在循环运动中保持粘连和凝聚的能力来制定的。


ASTM C732

Standard Test Method for Aging Effects of Artificial Weathering on Latex Sealants

This test method covers a laboratory procedure for the determination of aging effects of artificial weathering on latex sealants.


ASTM C732

乳胶密封剂人工老化试验效果的标准测试方法

该测试方法规定了测定人工老化乳胶密封剂老化效果的实验室程序。


ASTM C734

Standard Test Method for Low-Temperature Flexibility of Latex Sealants After Artificial Weathering

This test method covers a laboratory procedure for the determination of low-temperature flexibility of latex sealants after 500 h artificial weathering.


ASTM C734

人工老化后乳胶密封剂的低温弹性的标准测试方法

该测试方法规定了人工老化测试500小时后乳胶密封剂低温弹性的实验室程序。


ASTM C793

Standard Test Method for Effects of Laboratory Accelerated Weathering on Elastomeric Joint Sealants

This test method covers a laboratory procedure for determining the effects of accelerated weathering on cured-in-place elastomeric joint sealants (single- and multi-component) for use in building construction.


ASTM C793

弹性接缝密封胶实验室加速老化效果的标准测试方法

该测试方法包括了密封剂耐候性的测定,通过将密封剂经依据实验室加速老化程序反复暴露后,评价其在周期运动中保持粘合力和附着力。


ASTM D1148

Standard Test Method for Rubber Deterioration-Discoloration from Ultraviolet (UV) and Heat Exposure of Light-Colored Surfaces

This test method covers techniques to evaluate the surface discoloration of white or light-colored vulcanized rubber that may occur when subjected to UV or UV/visible exposure from specified sources under controlled conditions of relative humidity, or moisture, and temperature.


ASTM D1148

橡胶老化的标准测试方法-由紫外线(UV)和热曝露引起的浅色表面的变色

本测试方法规定了白色或浅色硫化橡胶表面变色的评估技术,受到指定来源的紫外线或紫外线/可见光照射,在受控的相对湿度或湿气及温度条件下,就有可能发生变色。


ASTM D1670

Standard Test Method for Failure End Point in Accelerated and Outdoor Weathering of Bituminous Materials

This test method covers the use of a spark generating apparatus for determination of failure due to cracking of bituminous materials undergoing accelerated or outdoor weathering on electrically conductive backings.


ASTM D1670

沥青材料加速和户外老化失效终点的标准测试方法

该测试方法规定了使用火花发生装置测定在导电底材上经加速或户外老化沥青材料的开裂失效。


ASTM D2565

Standard Practice for Xenon-Arc Exposure of Plastics Intended for Outdoor Applications

This practice covers specific procedures and test conditions that are applicable for xenon-arc exposure of plastics conducted in accordance with Practices G151 and G155.


ASTM D2565

户外用塑料氙灯曝露测试的标准测试方法

本测试方法依照G151和G155测试方法规定塑料氙灯曝露测试的具体程序和测试条件。


ASTM D3424

Standard Practice for Evaluating the Relative Lightfastness and Weatherability of Printed Matter

This standard describes procedures for the determination of the relative lightfastness and weatherability of printed matter under the following conditions, which involve exposure to natural daylight or accelerated procedures in the laboratory.


ASTM D3424

印刷品相对日晒色牢度和耐候性评估的标准测试方法

这个标准描述了印刷品在下列情况下相对日晒色牢度和耐候性的评估程序,涉及自然光曝露测试程序或实验室加速曝露测试程序。


ASTM D3451

Standard Guide for Testing Coating Powders and Powder Coatings

This guide covers the selection and use of procedures for testing coating powders and powder coatings. The test methods included are listed in Table 1. Where more than one test method is listed for the same characteristic, no attempt is made to indicate superiority of one method over another. Selection of the methods to be followed must be governed by experience and the requirements in each individual case, together with agreement between the purchaser and the seller.


ASTM D3451

涂料粉末和粉末涂料测试的标准指南

本指南规定了涂料粉末和粉末涂料测试的选择和使用程序。 测试方法已列于其中Table 1。对于某一特征,如果列出一个以上的测试方法,说明方法之间没有哪个更适合。 必须根据经验和每个案例的要求,以及买方和卖方之间的协议选择要遵循的方法。


ASTM D4101

Standard Specification for Polypropylene Injection and Extrusion Materials

This specification covers polypropylene materials suitable for injection molding and extrusion. Polymers consist of homopolymer, copolymers, and elastomer compounded with or without the addition of impact modifiers (ethylene-propylene rubber, polyisobutylene rubber, and butyl rubber), colorants, stabilizers, lubricants, or reinforcements.


ASTM D4101

聚丙烯注塑和挤出材料的标准规范

本规范规定了聚丙烯材料的注塑成型和挤出。 聚合物包括均聚物、共聚物及复合弹性体(加或不加聚异丁烯橡胶、乙丙橡胶、丁基橡胶等冲击改性剂),还有色素、稳定剂、润滑剂或增强剂。


ASTM D4303

Standard Test Methods for Lightfastness of Colorants Used in Artists' Materials

Four test methods to accelerate the effects of long term indoor illumination on artists' materials are described.


ASTM D4303

艺术材料中使用的着色剂光稳定性的标准测试方法

描述了4种加速长期室内照明对艺术材料的影响的测试方法。


ASTM D4355

Standard Test Method for Deterioration of Geotextiles by Exposure to Light, Moisture and Heat in a Xenon Arc Type Apparatus

This test method covers the determination of the deterioration in tensile strength of geotextiles by exposure to xenon arc radiation, moisture, and heat.


ASTM D4355

曝露在氙灯设备的光、潮湿和热中的土工布老化的标准测试方法

该测试方法规定了曝露在氙灯辐射、湿气和热量中的土工布拉伸强度退化的测定。


ASTM D4434

Standard Specification for Poly(Vinyl Chloride) Sheet Roofing

This specification covers flexible sheet made from poly(vinyl chloride) resin as the primary polymer intended for use in single-ply roofing membranes exposed to the weather.


ASTM D4434

聚氯乙烯屋面薄板的标准规范

本规范规定了拟用于单层屋顶薄膜的、用聚氯乙烯树脂作为初级聚合物而制造的柔性薄板空气暴露测试程序。


ASTM D4459

Standard Practice for Xenon-Arc Exposure of Plastics Intended for Indoor Applications

This practice covers specific procedures and test conditions that are applicable for exposure of plastics in window glass-filtered xenon-arc devices in accordance with Practices G151 and G155 for evaluating the stability of plastics intended for use in indoor applications.


ASTM D4459

室内用塑料氙灯曝露测试的标准测试方法

本测试方法规定了依照测试方法G151和G155,用配备窗玻璃滤光器的氙灯设备对塑料进行暴露测试的具体程序和测试条件,以评估室内用塑料的稳定性。


ASTM D4637

Standard Specification for EPDM Sheet Used In Single-Ply Roof Membrane

This specification covers flexible sheet made from ethylene-propylene-diene terpolymer (EPDM) intended for use in single-ply roofing membranes exposed to the weather.


ASTM D4637

用于单层屋顶薄膜的EPDM薄板的标准规范

本规范规定了拟用于单层屋顶薄膜的用乙烯丙烯三元共聚物(EPDM)制造的柔性薄板在空气中的曝露测试程序。


ASTM D4798

Standard Practice for Accelerated Weathering Test Conditions and Procedures for Bituminous Materials (Xenon-Arc Method)

This practice covers test conditions and procedures for xenon-arc exposures according to Practices G151 and G155 for bituminous roofing and waterproofing materials.


ASTM D4798

沥青材料(氙弧法)加速老化测试条件和测试程序的标准测试方法

本测试方法规定了根据G151和G155沥青屋面和防水材料的做法进行氙灯曝露测试的测试条件和程序。


ASTM D4811

Standard Specification for Nonvulcanized (Uncured) Rubber Sheet Used as Roof Flashing

This specification covers nonvulcanized (uncured) rubber sheet made of EPDM (ethylene-propylene-diene terpolymer) or CR (polychloroprene) intended for use as watertight roof flashing exposed to the weather.


ASTM D4811

用作屋面防雨板的非硫化(未固化)橡胶薄板的标准规范

本规范规定了由EPDM(乙烯丙烯三元共聚物)或CR(氯丁橡胶)制成的、拟用于防水屋面防雨板的非硫化(未固化)橡胶薄板在空气中的曝露测试。


ASTM D5019

Standard Specification for Reinforced CSM (Chlorosulfonated Polyethylene) Sheet Used in Single-Ply Roof Membrane

This specification covers reinforced non-vulcanized polymeric sheet made from chlorosulfonated polyethylene (CSM) intended for use as a single-ply roof membrane exposed to the weather.


ASTM D5019

用于单层屋顶薄膜的增强CSM板(氯磺化聚乙烯)的标准规范

本规范规定了拟用于单层屋顶薄膜的、用氯磺化聚乙烯(CSM)制造的增强非硫化聚合物板空气曝露测试程序。


ASTM D5071

Standard Practice for Exposure of Photodegradable Plastics in a Xenon Arc Apparatus

This practice covers specific procedures and test conditions that are applicable for xenon arc exposure of photodegradable plastics conducted in accordance with Practices G151 and G155.


ASTM D5071

氙灯装置中光降解塑料曝露测试的标准测试方法

本测试方法规定了依照G151和G155测试方法对塑料进行光降解氙灯曝露测试的具体程序和测试条件。


ASTM D5383

Standard Practice for Visual Determination of the Lightfastness of Art Materials by Art Technologists

This practice covers a method for exposing specimens of colored art materials indoors to sunlight coming through a closed window.


ASTM D5383

艺术材料日晒色牢度目测标准测试方法

本测试方法规定了室内彩色艺术材料样品曝露于透过封闭窗玻璃的太阳光中的测试。


ASTM D5398

Standard Practice for Visual Evaluation of the Lightfastness of Art Materials by the User

This practice covers a method for exposing specimens of colored art materials indoors to sunlight coming through a closed window.


ASTM D5398

用户对艺术材料日晒色牢度目测评估的测试方法

本测试方法规定了室内彩色艺术材料样品曝露于透过封闭窗玻璃的太阳光中的测试。


ASTM D5819

Standard Guide for Selecting Test Methods for Experimental Evaluation of Geosynthetic Durability

This guide covers a designer/specifier through a systematic determination of those factors of the appropriate application environment that may affect the post-construction service life of a geosynthetic.


ASTM D5819

土工合成材料耐候性测试评估方法选择的标准指南

本指南系统地设计/明确了可能影响土工合成材料施工后的使用寿命的环境因素。


ASTM D6083

Standard Specification for Liquid Applied Acrylic Coating Used in Roofing

This specification covers liquid-applied water-dispersed acrylic latex elastomeric protective roof coatings.


ASTM D6083

屋顶用液态丙烯酸涂料标准规范

本规范描述了液态水分散型丙烯酸乳液橡胶屋顶防护涂料。


ASTM D6551

Standard Practice for Accelerated Weathering of Pressure-Sensitive Tapes by Xenon-Arc Exposure Apparatus

This practice describes one environment for the exposure of pressure-sensitive tape, used primarily for packaging, to a laboratory accelerated weathering environment.


ASTM D6551

使用氙灯曝露装置对与压力敏感的带材进行加速老化的标准测试方法

本测试方法描述了实验室加速老化环境下对与压力敏感的带材进行曝露测试,主要用于包装材料。


ASTM D6551

使用氙灯曝露装置对与压力敏感的带材进行加速老化的标准测试方法

本测试方法描述了实验室加速老化环境下对与压力敏感的带材进行曝露测试的程序,主要用于包装材料。


ASTM D6577

Standard Guide for Testing Industrial Protective Coatings

This guide covers the selection and use of test methods and procedures for testing industrial protective coatings.


ASTM D6577

工业防护涂料测试标准指南

本指南规定了工业防护涂料测试方法和测试程序的选择和使用。


ASTM D6662

Standard Specification for Polyolefin-Based Plastic Lumber Decking Boards

This specification covers polyolefin-based plastic lumber products for use as exterior residential decking boards.


ASTM D6662

聚烯烃基木塑装饰板的标准规范

本规范规定了住宅外墙板用聚烯烃塑料板材的使用。


ASTM D6695

Standard Practice for Xenon-Arc Exposures of Paint and Related Coatings

This practice covers the selection of test conditions for accelerated exposure testing of coatings and related products in xenon arc devices conducted according to Practices G151 and G155.


ASTM D6695

油漆及相关涂料氙灯曝露测试的标准测试方法

本测试方法规定了涂料及相关产品在氙灯设备中根据G151 和 G155测试方法进行加速曝露测试时对测试条件的选择。


ASTM D6878

Standard Specification for Thermoplastic Polyolefin Based Sheet Roofing

This specification covers flexible sheet made from thermoplastic polyolefin (TPO) as the principal polymer, intended for use in single-ply roofing membranes exposed to the weather.


ASTM D6878

基于热塑性聚烯烃的屋顶板标准规范

本规范规定了拟用于单层屋顶薄膜的、用热塑性聚烯烃(TPO)作为主要聚合物而制造的柔性板空气暴露测试程序。


ASTM D7356

Standard Test Method for Accelerated Acid Etch Weathering of Automotive Clearcoats Using a Xenon-Arc Exposure Device

This test method covers an accelerated exposure test intended to simulate defects in automotive clearcoats caused by acid rain that occurs at the Jacksonville, Florida exposure site.


ASTM D7356

使用氙灯暴露设备对汽车面漆进行加速酸蚀老化的标准测试方法

本测试方法旨在模拟发生在佛罗里达曝晒场杰克逊维尔的因酸雨造成的汽车清漆破坏的加速暴露测试。


ASTM D750

Standard Test Method for Rubber Deterioration Using Artificial Weathering Apparatus

This test method covers specific variations in the test conditions and procedures that shall be applicable when Practice G151 plus either Practice G152, G153, G154, or G155 are employed for exposure of vulcanized rubber compounds.


ASTM D750

使用人工老化设备对橡胶进行老化试验的标准测试方法

本测试方法规定了可用的测试条件和测试程序的具体变化,在进行硫化橡胶复合物曝露测试时,可采用测试方法G151和G152、G153、G154、G155中的任意一个。


ASTM D7869

Standard Practice for Xenon Arc Exposure Test with Enhanced Light and Water Exposure for Transportation Coatings

This test procedure is used to simulate the physical and environmental stresses that a coating for exterior transportation applications (for example, automotive) is exposed to in a subtropical climate, such as southern Florida.


ASTM D882

Standard Test Method for Tensile Properties of Thin Plastic Sheeting

This test method covers the determination of tensile properties of plastics in the form of thin sheeting and films (less than 1.0 mm (0.04 in.) in thickness).


ASTM D882

薄塑料板拉伸性能的标准测试方法

本测试方法规定了薄片和薄膜(小于1毫米(0.04英寸)厚度)塑料拉伸性能的测定。


ASTM D904

Standard Practice for Exposure of Adhesive Specimens to Artificial Light

This practice covers the basic principles and operating procedures for ultraviolet (UV) light aging (with or without water) of adhesive bonded joints having at least one glass or transparent adhered, using fluorescent UV (see Method A) or xenon-arc light sources (see Method B).


ASTM D904

人工光源胶粘剂样品暴露的标准测试方法

本测试方法规定了胶接接头(至少有一个玻璃或透明粘接)紫外线(UV)光老化(有水循环或无水循环)的基本原则和操作程序,使用荧光紫外线(见方法A)或氙弧光源(见方法B)。


ASTM D925

Standard Test Methods for Rubber Property—Staining of Surfaces (Contact, Migration, and Diffusion)

These test methods cover techniques to evaluate three types of staining that rubber may cause when in contact with, or in proximity to, another surface that may be light colored.


ASTM D925

橡胶性能——表面染色(接触、迁移、扩散)的标准测试方法

这些测试方法规定了评估橡胶材料接触或靠近其他浅色表面产生的三种沾色的技术。


ASTM F1164

Standard Test Method for Evaluation of Transparent Plastics Exposed to Accelerated Weathering Combined with Biaxial Stress

This test method covers the resistance of transparent plastics exposed to environmental conditioning (accelerated weathering) under a biaxial stress state induced by a pressure cell/test fixture.


ASTM F1164

透明塑料受到双轴应力与加速老化暴露评估的标准测试方法

本测试方法规定了透明塑料在压力部件/测试支架导致的双轴应力状态下曝露于环境条件(加速老化)的抵抗力。


ASTM F1515

Standard Test Method for Measuring Light Stability of Resilient Flooring by Color Change

This test method provides a means of measuring the amount of color change in flooring products when subjected to accelerated light exposure over a period of time (functional use of the flooring product).


ASTM F2366

Standard Practice for Determining the Relative Lightfastness of Ink Jet Prints Exposed to Window Filtered Daylight Using a Xenon Arc Light Apparatus

This practice covers specific procedures and test conditions that are applicable for xenon-arc exposure of ink jet media prints conducted in accordance with Practices G151 and G155.


ASTM F2366

使用配备窗玻璃滤光器的氙灯设备测试喷墨印刷品的相对光稳定性的标准测试方法

本测试方法规定了依照G151和G155测试方法对喷墨纸张印刷品进行氙灯曝露测试的具体程序和测试条件。


ASTM G151

Practice for Exposing Nonmetallic Materials in Accelerated Test Devices That Use Laboratory Light Sources

This practice provides general procedures to be used when exposing nonmetallic materials in accelerated test devices that use laboratory light sources.


ASTM G151

使用实验室光源加速测试设备对非金属材料进行曝露的测试方法

本测试方法提供了在实验室光源加速测试设备中对非金属材料进行曝露测试的一般程序。


ASTM G155

Practice for Operating Xenon Arc Light Apparatus for Exposure of Non-Metallic Materials

This practice covers the basic principles and operating procedures for using xenon arc light and water apparatus intended to reproduce the weathering effects that occur when materials are exposed to sunlight (either direct or through window glass) and moisture as rain or dew in actual use.


ASTM G155

使用氙灯设备对非金属材料进行曝露的测试方法

本测试方法是使用氙灯和水喷淋装置进行曝露测试的基本原则和操作程序,旨在再现材料曝露在阳光下(直接或透过窗玻璃)和曝露在湿气中(雨水或露水)发生的老化效果。


GB 6806

Anodizing of aluminium and its alloys--Accelerated test of light fastness of coloured anodic oxide coatings using artificial light

This standard specifies the artificial light accelerated test method for evaluating the light resistance of aluminum and aluminum alloy colored anodized films.


GB/T 16259

Test method for in accelerated weathering building materials

This standard specifies the content, test conditions, test procedures, test results, and test reports of artificial climate accelerated aging test devices using xenon lamps as the light source for building material products.


GB/T 16422.1

Plastics-Methods of the exposure to laboratory light sources Part 1:general guidance

This part of GB / T 16422 provides information and general principles on the selection and implementation of exposure methods described in detail in the following sections. It also describes and recommends methods for measuring irradiance and radiant quantities, and describes monitoring boxes. Equipment requirements for body air temperature and surface temperature of dark and light colored materials.


GB/T 16422.2

Plastics - Methods of exposure to laboratory light sources - Part 2: Xenon-arc sources

This part of GB / T 16422 specifies the test method for plastic samples exposed to xenon arc lamps in the presence of moisture. This method is used to simulate the natural occurrence of materials in sunlight in the actual use environment after exposure to sunlight or filter glass Aging effect.


GB/T 16991

Textiles - Test for colour fastness - Colour fastness and ageing to artificial light at high temperatures: Xenon arc

This standard specifies a method for determining the color of various types of textiles, the ability of artificial light sources to replace natural sunlight, the ability to resist heat, and the ability to resist aging. This test method specifically takes into account the effects of light and heat generated by the interior of the vehicle on the textile.


GB/T 1710

Comparison of resistance to light of coloured pigments of similar types

This standard specifies a general test method for the comparison of light fastness of the same type of pigments (agreed reference pigments and test samples).
            


GB/T 18244

Test methods for resistance to weathering of building waterproofing materials

This standard specifies test methods for hot air aging, ozone aging, and artificial climate accelerated aging (xenon arc lamps, carbon arc lamps, ultraviolet fluorescent lamps).


GB/T 1865

Paints and varnishes - Artificial weathering and exposure to artificial radiation - Exposure to filtered xenon-arc radiation

This standard specifies artificial weathering test procedures for paints and varnishes exposed to xenon lamp devices and water and water vapor. The results of aging can be individually evaluated by comparing the parameters selected before, during and after aging.


GB/T 22771

Graphic techmology-Prints and printing inks-Assessment of light fastness using filtered xenon arc light

This standard specifies a method for determining the light resistance of printed matter and printing inks. It gives two test conditions: basic test conditions for printed matter and special test conditions for ink.


GB/T 2423.24

Environmental testing for electric and electronic products Part 2:Test methods-Test Sa: simulated solar radiation at ground level

This standard is used to test the impact of ground solar radiation on equipment and components (thermal, mechanical, chemical, electrical, etc.)


GB/T 29365

Wood-plastic composite (WPC) – test methods of artificial weathering

This standard specifies the artificial weathering test method for plastic-wood composite materials.


GB/T 32088

Accelerated weathering test methods of automotive nonmetal components and materials using a xenon-arc apparatus

This standard specifies the test method and evaluation method for accelerating aging of automotive non-metal parts and materials using controlled irradiance xenon equipment.


GB/T 8427

Textiles-Tests for colour fastness-Colour fastness to artifical light:Xenon arc fading lamp test

This standard specifies a method to determine the color fastness of various types of textiles to the artificial light effect equivalent to sunlight (D65). This standard can also be used for white (bleached or fluorescent whitened) textiles.


GM 9125P

Procedures for Laboratory Accelerated Exposure of Automotive Materials

These procedures are used to determine the resistance to degradation of automotive materials when subjected to artificial light sources. It describes exposures to sunshine carbon arc, xenon arc, fluorescent ultraviolet light and condensation apparatus, and a twin carbon arc.


GM 9125P

汽车材料实验室加速老化测试程序

这些程序用于测定受到人造光源照射时汽车材料的抗降解能力。 它描述了日光型碳弧、氙弧、荧光紫外线和冷凝装置和双碳弧的暴露测试。


IEC 61345

UV Test for Photovaltalic (PV) Modules


IEC 61345

光伏组件(PV)紫外试验


ISO 105-B02 (EN) (DIN)

Textiles-Tests for colour fastness- Part B02: Colour fastness to artificial light: Xenon arc fading lamp test


ISO 105-B02 (EN) (DIN)

纺织品-日晒色牢度试验-B02部分:人造光色牢度: 氙弧灯


ISO 105-B04 (EN) (DIN)

Textiles - Tests for Colour Fastness - Part B04. Colour Fastness to Artificial Weathering: Xenon Arc Fading Lamp Test


ISO 105-B06 (EN) (DIN)

Textiles - Tests for Colour Fastness - Part B06: Colour Fastness and Ageing to Artificial Light at High Temperatures: Xenon Arc Fading Lamp Test


ISO 105-B07 (EN) (DIN)

Textiles - Tests for Colour Fastness - Part B07: Colour Fastness to Light of Textiles Wetted with Artificial Perspiration


ISO 105-B10 (EN) (DIN)

Textiles - Tests for Colour Fastness - Part B10: Artificial Weathering - Exposure to Filtered Xenon-Arc Radiation


ISO 12040

Graphic Technology - Prints and Printing Inks - Assessment of Light Fastness Using Filtered Xenon Arc Light


ISO 12040

图形技术-印刷品和印刷油墨-用过滤氙弧灯评估光稳定性


ISO 16474-2

Paints and varnishes — Methods of exposure to laboratory light sources — Part 2: Xenon-arc lamps


ISO 29664

Plastics - Artificial weathering including acidic deposition


ISO 4892-1 (EN) (DIN)

Plastics – Methods of Exposure to Laboratory Light Sources – Part 1: General guidance


ISO 4892-1 (EN) (DIN)

塑料–使用实验室光源进行曝露测试的方法–第一部分 一般指导


ISO 4892-2 (EN) (DIN)

Plastics - Methods of Exposure to Laboratory Light Sources - Part 2: Xenon-arc lamps


ISO 4892-2 (EN) (DIN)

塑料–使用实验室光源进行曝露测试的方法–第二部分 氙弧灯


QB/T 2727

Leather-Tests for colour fastness-colour fastness to artificial light: Xenon arc

This standard specifies the test method for the color of leather against artificial light sources and heat resistance.


QB/T 4873

Test methods of artificial leather and synthetic leather - Exposure to laboratory light sources

This standard specifies three methods for the light source exposure test of artificial leather and synthetic leather laboratories: xenon arc lamp method (A method), fluorescent ultraviolet lamp method (B method), and open carbon arc lamp method (C method), and their results and Evaluation.


SAE J2412

使用可控辐照度的氙灯设备对汽车内饰件进行加速曝露测试


该测试方法描述了受控辐照度的氙灯装置用于各种汽车内饰件加速曝露测试的操作程序


SAE J2412

Accelerated Exposure of Automotive Interior Trim Components Using a Controlled Irradiance Xenon-Arc Apparatus

This test method specifies the operating procedures for a controlled irradiance, xenon arc apparatus used for the accelerated exposure of various automotive interior trim components.


SAE J2527

Performance Based Standard for Accelerated Exposure of Automotive Exterior Materials Using A Controlled Irradiance Xenon-Arc Apparatus

This SAE Standard specifies the operating procedures for a controlled irradiance, xenon-arc apparatus used for the accelerated exposure of various exterior automotive materials.


SAE J2527

使用可控辐照度的氙灯设备对汽车外饰材料进行加速曝露的测试标准

本SAE标准描述了受控辐照度的氙灯装置用于各种汽车外饰材料加速曝露测试的操作程序。


T/CSAE 104

Laboratory xenon arc exposure test method of automotive exterior decoration coatings

This standard specifies the test method for accelerated aging of automotive exterior coatings using controlled irradiance xenon lamp equipment.


VW PV 1306

Exposure Test for Determining the Tackiness of Polypropylene Parts


VW PV 1306

测定聚丙烯零件粘性的曝露测试


VW PV 3929

Non-Metallic Materials, Weathering in Dry, Hot Climate


VW PV 3929

非金属材料在干、热气候环境中的老化


VW PV 3930

Non-Metallic Materials, Weathering in Moist, Hot Climate


VW PV 3930

非金属材料在湿、热气候环境中的老化


YC/T 374

Printed cigarette carton and packet packaging papers - conformity test for color fastness to light - xenon arc fading lamp test

This standard specifies the test method for the lightfastness and fastness of cigarette rods and carton paper.


YY/T 0631

dental materials - determination of color stability

This standard specifies the method for determining the color stability of dental materials after immersion in light.


Looking for a specific test standard? Search entire listing of all standards.

 

资源

联系我们

Q-Lab 电话号码

美国:+1-440-835-8700
佛罗里达及亚利桑那企业管理:+1-305-245-5600
英国/欧洲:+44-1204-861616
德国:+49-681-857470
中国:+86-21-5879-7970

 