Test Standards for Arizona Outdoor Exposure Testing
AAMA 2603
Voluntary Specification, Performance Requirements and Test Procedures For Pigmented Organic Coatings on Aluminum Extrusions and Panels
This specification describes test procedures and performance requirements for pigmented organic coatings applied to aluminum extrusions and panels.
AATCC TM111
Weather Resistance of Textiles: Exposure to Daylight and Weather
This test method provides a means for determining the weather resistance of textile materials.
ASTM C1589
Standard Practice for Outdoor Weathering of Construction Seals and Sealants
This practice describes outdoor exposure procedures used to determine the weathering durability of building construction, seals and sealants.
ASTM D1006
Standard Practice for Conducting Exterior Exposure Tests of Paints on Wood
This practice covers procedures to be followed for direct exposure of house and trim paints on new, previously unpainted wood materials to the environment.
ASTM D1014
Standard Practice for Conducting Exterior Exposure Tests of Paints and Coatings on Metal Substrates
This practice covers procedures to be followed for direct exposure of exterior paints and coatings to the environment when applied to metal surfaces.
ASTM D1435
Standard Practice for Outdoor Weathering of Plastics
This practice is intended to cover procedures for the exposure of plastic materials to weather. Note 1See Practice G 24 for aging under glass.
ASTM D1670
Standard Test Method for Failure End Point in Accelerated and Outdoor Weathering of Bituminous Materials
This test method covers the use of a spark generating apparatus for determination of failure due to cracking of bituminous materials undergoing accelerated or outdoor weathering on electrically conductive backings.
ASTM D3424
Standard Practice for Evaluating the Relative Lightfastness and Weatherability of Printed Matter
This standard describes procedures for the determination of the relative lightfastness and weatherability of printed matter under the following conditions, which involve exposure to natural daylight or accelerated procedures in the laboratory.
ASTM D3679
Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Siding
This specification establishes requirements and test methods for the materials, dimensions, warp, shrinkage, impact strength, expansion, appearance, and windload resistance of extruded single-wall siding manufactured from rigid (unplasticized) PVC compound. Methods of indicating compliance with this specification are also provided.
ASTM D4101
Standard Specification for Polypropylene Injection and Extrusion Materials
This specification covers polypropylene materials suitable for injection molding and extrusion. Polymers consist of homopolymer, copolymers, and elastomer compounded with or without the addition of impact modifiers (ethylene-propylene rubber, polyisobutylene rubber, and butyl rubber), colorants, stabilizers, lubricants, or reinforcements.
ASTM D4303
Standard Test Methods for Lightfastness of Colorants Used in Artists' Materials
Four test methods to accelerate the effects of long term indoor illumination on artists' materials are described.
ASTM D4726
Standard Specification for Rigid Poly(Vinyl Chloride) (PVC) Exterior-Profile Extrusions Used for Assembled Windows and Doors
This specification establishes requirements for the material properties, including dimensional stability, weatherability, and extrusion quality, of rigid poly(vinyl chloride) (PVC) exterior profile extrusions used for assembled windows and doors.
ASTM D5272
Standard Practice for Outdoor Exposure Testing of Photodegradable Plastics
This practice defines test conditions applicable when Practices D1435 and G7 are employed for the outdoor exposure testing of photodegradable plastics.
ASTM D5722
Standard Practice for Performing Accelerated Outdoor Weathering of Factory- Coated Embossed Hardboard Using Concentrated Natural Sunlight and a Soak-Freeze-Thaw Procedure
This practice covers techniques to accelerate weathering effects of factory-coated embossed hardboard using Cycle 1 of Practice G90 (concentrated natural sunlight with periodic surface water spray) plus a soak-freeze thaw cycle.
ASTM D5819
Standard Guide for Selecting Test Methods for Experimental Evaluation of Geosynthetic Durability
This guide covers a designer/specifier through a systematic determination of those factors of the appropriate application environment that may affect the post-construction service life of a geosynthetic.
ASTM D5970
Standard Test Method for Deterioration of Geotextiles from Outdoor Exposure
This test method covers evaluating the deterioration in tensile strength and strain after outdoor exposure.
ASTM D6662
Standard Specification for Polyolefin-Based Plastic Lumber Decking Boards
This specification covers polyolefin-based plastic lumber products for use as exterior residential decking boards.
ASTM D6864
Standard Specification for Color and Appearance Retention of Solid Colored Plastic Siding Products
This specification establishes requirements and test methods for the color and appearance retention of solid colored plastic siding products.
ASTM D7251
Standard Specification for Color and Appearance Retention of Variegated Color Plastic Siding Products
This specification establishes requirements and test methods for the color and appearance retention of variegated color plastic siding products.
ASTM E782
Standard Practice for Exposure of Cover Materials for Solar Collectors to Natural Weathering Under Conditions Simulating Operational Mode
This practice provides a procedure for the exposure of cover materials for flat-plate solar collectors to the natural weather environment at temperatures that are elevated to approximate operating conditions.
ASTM E881
Standard Practice for Exposure of Solar Collector Cover Materials to Natural Weathering Under Conditions Simulating Stagnation Mode
This practice covers a procedure for the exposure of solar collector cover materials to the natural weather environment at elevated temperatures that approximate stagnation conditions in solar collectors having a combined back and edge loss coefficient of less than 1.5 W/(m2 · °C).
ASTM F1164
Standard Test Method for Evaluation of Transparent Plastics Exposed to Accelerated Weathering Combined with Biaxial Stress
This test method covers the resistance of transparent plastics exposed to environmental conditioning (accelerated weathering) under a biaxial stress state induced by a pressure cell/test fixture.
ASTM F2657
Standard Test Method for Outdoor Weathering Exposure of Crosslinked Polyethylene (PEX) Tubing
This test method describes the procedure for exposing crosslinked polyethylene (PEX) tubing produced in accordance with Specification F 876 to natural (sunlight) ultraviolet (UV) radiation and evaluating the effects of the exposure.
ASTM G201
Standard Practice for Conducting Exposures in Outdoor Glass-Covered Exposure Apparatus with Air Circulation
This practice covers the basic principles and operating procedures for using outdoor glass-covered exposure apparatus with air circulation.
ASTM G24
Standard Practice for Conducting Exposures to Daylight Filtered Through Glass
This practice evaluates the resistance of nonmetallic materials to solar radiation filtered through glass.
ASTM G50
Standard Practice for Conducting Atmospheric Corrosion Tests on Metals
This practice covers and defines conditions for exposure of metals and alloys to the weather. It sets forth the general procedures that should be followed in any atmospheric test. It is presented as an aid in conducting atmospheric corrosion tests so that some of the pitfalls of such testing may be avoided. As such, it is concerned mainly with panel exposures to obtain data for comparison purposes.
ASTM G7
Standard Practice for Atmospheric Environmental Exposure Testing of Nonmetallic Materials
This practice covers procedures to be followed for direct exposure of nonmetallic materials to the environment. When originators of a weathering test have the actual exposure conducted by a separate agency, the specific conditions for the exposure of test and control specimens must be clearly defined and mutually agreed upon between all parties.
EN 12224 (DIN)
Geotextiles and Geotextile-Related Products - Determination of the Resistance to Weathering
EN 13523-19 (DIN)
Coil Coated Metals - Test Methods Part 19: Panel Design and Method of Atmospheric Exposure Testing
Ford DVM0020
Outdoor Weathering Tests
This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.
Ford FLTM BI 160-01
Florida and Arizona Outdoor Exposure Test
GM 2617M
Interior Trim Parts Performance
This specification covers the performance requirements of instrument panels, consoles, door trim, quarter trim panel, garnish moldings, armrests, headrests, assist handles, rear window trim panel and seat trims.
GM 3619M
Flexible Laminating Films and Film Plastic Laminates
This specification details the requirements for flexible plastic films that may be laminated to either metal or plastic substrates.
GM 7454M
Soft Interior Trim Parts
This standard covers the performance and approval requirements for three classes of soft interior trim parts.
GM 7455M
Decorative Interior Plastic Laminates and Films
This specification gives the durability requirements for plastic parts decorated with wood grains, or patterns for interior trim panels. The materials shall be classified into four types.
GM 9538P
Weathering Exposure Tests For Interior Trims
This specification describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies.
GMW 14873
Outdoor Weathering of Automotive Exterior Materials
GMW 3417
Natural Weathering Exposure Tests for Interior Trims/Materials
This test procedure describes procedures for conducting natural weathering exposure tests to evaluate the exposure tolerance of interior automotive materials, components, and assemblies. The tests are conducted in climatic regions which offer extreme solar environments.
ISO 2810 (EN) (DIN)
Paints and Varnishes - Notes for Guidance on The Conduct of Natural Weathering Tests
ISO 877-1 (EN) (DIN)
Plastics - Methods of Exposure to Solar Radiation - Part 1: General Guidance
ISO 877-2 (EN) (DIN)
Plastics - Methods of Exposure to Solar Radiation - Part 2: Direct Weathering and Exposure Behind Window Glass
SAE J1976
Outdoor Weathering of Exterior Materials
Looking for a specific test standard? Search entire listing of all standards.
You are now logged in to your account. You can now freely access all (
) or (
) documents. To access (
) documents, please register your equipment here.
You are now logged in to your account. You can now freely access all (
) or (
) documents. To access (
) documents, please register your equipment here.
Create an Account
Learn more about creating an account with Q-Lab