LF-8147 Marine Performance from Salt Fog
      
             
                          This article presents a brief description of the various approaches to determine longterm durability of coatings. Following the introduction, some data from SSPC's Performance of Alternate Coatings in the Environment (PACE) program are presented, com...
              