Products

Contact Us

  1.  

Q-Lab Phone Numbers

USA: +1-440-835-8700
Florida: +1-305-245-5600
Arizona: +1-623-386-5140
UK/Europe: +44-1204-861616
Germany: +49-681-857470
China: +86-21-5879-7970

Q-FOG Cyclic Corrosion Tester
Click to Enlarge Image
Q-FOG Cyclic Corrosion Tester corrosion chamber test holders corrosion test panel holders ccorrosion test chambers Q-FOG-Bubble-Tower Q-FOG specimen area how corrosion chamber works Q-FOG How it works 1 Q-FOG How it works 2 Q-FOG How it works 3
Click to Switch Image

Q-FOG Cyclic Corrosion Tester

Cyclic corrosion testing provides the best possible laboratory simulation of natural atmospheric corrosion. Research indicates that test results are similar to outdoors in resulting structure, morphology, and relative corrosion rates.

Q-FOG cyclic corrosion chambers from Q-Lab can run traditional salt spray, Prohesion, and most cyclic automotive tests. Q-FOG chambers are available in two sizes to fulfill a wide range of testing requirements.

Q-FOG cyclic corrosion testers are the simplest, most reliable, and easiest to use corrosion testers available.


Cyclic Corrosion Testing
Prior to cyclic corrosion testing, conventional salt spray (a continuous salt spray at 35˚C), was the standard way to simulate corrosion in a lab.   Because conventional salt spray methods failed to mimic the natural wet/dry cycles of the outdoors, test results frequently provided poor correlation to outdoors. 

In a Q-FOG cyclic corrosion tester, specimens are exposed to a series of different environments in a repetitive cycle that mimics the outdoors.  Simple cycles, such as Prohesion, may consist of cycling between salt fog and dry conditions.  More sophisticated automotive methods may call for multi-step cycles that incorporate humidity or condensation, along with salt spray and dry-off.  

Within one Q-FOG chamber, it is possible to cycle through a series of the most significant corrosion environments.  Even extremely complex test cycles can easily be programmed with the Q-FOG controller. See LF8110 - Q-FOG Specifications or visit our standards page for a detailed list of test methods met by the Q-FOG chamber. 

Q-FOG corrosion test chambers are available in two types. Model SSP performs traditional salt spray and Prohesion tests. Model CCT performs salt spray, Prohesion, and 100% humidity for most cyclic automotive tests.


Easy Programming and Sample Mounting

The Q-FOG test chamber is designed to cycle between four conditions: Fog, Dry-Off, 100% Humidity (Model CCT only), and Dwell.  Test conditions, time, and temperature are controlled by a built-in microprocessor.  A remarkably simple user interface allows for easy user programming and operation.  The operator can quickly create new cycles, or run any of the programmed cycles.  The Q-FOG controller includes complete self-diagnostics, including warning messages, routine service reminders and safety shut down.

The Q-FOG tester has a low belt line and an easy opening lid for easy sample mounting.  The SSP-600 and CCT-600 models have a capacity of about 160 test panels of 75mm x 150mm in size.  The SSP-1100 and CCT-1100 models have a capacity of 240 test panels.

Precise Control of Fog Dispersion
The Q-FOG cyclic corrosion chamber has superior fog dispersion compared to conventional systems, which cannot vary volume and distance independently.  A variable speed peristaltic pump controls the amount of corrosive solution delivered to the spray atomizer, while the air pressure regulator controls the distance of the “throw.”  Note that purified water is required for proper operation of Q-FOG corrosion testers.

Internal Solution Reservoir
Space utilization is maximized and maintenance is minimized with the Q-FOG tester's internal solution reservoir. The 120 liter reservoir has enough capacity for running most tests for 7 days or more. The reservoir has an integral salt filter and a built-in alarm to alert the operator when the solution is low.

Fast Cycling

Q-FOG testers can change temperatures exceptionally fast because of their unique internal chamber heater and their high volume cooling/dry-off blower. An additional air heater allows very low humidity dry-off exposures. Conventional chambers with water jackets cannot cycle rapidly because of the thermal mass of the water, nor can they produce low humidity.

Affordable

Q-FOG cyclic corrosion testers offer state of the art corrosion testing technology, reliability, ease of operation and easy maintenance – all at a remarkably affordable price.


Models
(also see Features Tab)

  • Q-FOG SSP-600: conventional salt spray and Prohesion tests, 640 liter chamber volume
  • Q-FOG SSP-1100: conventional salt spray and Prohesion tests, 1103 liter chamber volume
  • Q-FOG CCT-600:  conventional salt spray, Prohesion, and 100% humidity, 640 liter chamber volume
  • Q-FOG CCT-1100: conventional salt spray, Prohesion, and 100% humidity, 1103 liter chamber volume

See LF-8110 - Q-FOG Specifications for comparative information, or see the Features Tab.

    Model SSP for Prohesion or Conventional Salt Spray Tests
    Numerous accelerated corrosion tests may be performed in Q-FOG SSP corrosion tester including Prohesion, ASTM B117 and G85, BS 3900 F4 & F9, DIN 50.021 and ISO 9227.  Visit our standards page or see LF-8131 - Partial List of Standards Met by Q-FOG for more information.

      The Prohesion test uses fast cycling, rapid temperature changes, a low humidity dry-off cycle and a different corrosive solution to provide a more realistic test.  Many researchers have found this test useful for industrial maintenance coatings.

      Continuous salt spray exposures are widely specified for testing components and coatings for corrosion resistance.  Applications include plated and painted finishes, aerospace and military components, and electrical/electronic systems.

      Most of these tests are performed to particular specifications such as ASTM B117 (Salt Spray), and BS 3900 F4. These tests are widely used for relative corrosion testing.  They are typically run at an elevated temperature and do not incorporate a dry-off cycle.  They require heated, humidified air for the spray.

      Model CCT for Corrosion Research and Cyclic Automotive Tests
      The Q-FOG model CCT has all the advantages of the model SSP, but adds the flexibility of including 100% humidity.
      Today’s automotive corrosion test methods typically call for exposing specimens to a repetitive cycle of salt spray, high humidity, low humidity dry-off, and ambient conditions. These test methods were originally developed as labor intensive manual procedures.  The multi-functional Q-FOG CCT corrosion tester is designed to perform these cyclic tests automatically in a single chamber.

      Q-FOG model CCT advantages include the elimination of:

      • manual moving of test specimens from one chamber to another
      • laborious spraying of test specimens
      • variability in results from excessive specimen handling

      Model CCT units come equipped with a viewing window in the side of the lid and an internal light to allow easy monitoring of the test conditions.

      Specimen Holders
      Optional test panel holders are available which allow the user to mount specimens at a 15 degree angle, holding panels up to 102mm x 304mm on 38mm centers.

      Odd shaped parts (e.g. large three-dimensional specimens), can be mounted on special 20mm hanging rods.  See our specimen mounting page, LF-8151 - Q-FOG Specimen Mounting, or inquire about the following common part numbers:

      • F-9008-K    Q-FOG SSP-600 or CCT-600 Test Panel Holder Kit, set of 8
      • F-9011-K    Q-FOG SSP-1100 or CCT-1100 Test Panel Holder Kit, set of 10
      • F-9014-K    Q-FOG SSP-600 or CCT-600 20mm (3/4”) Hanging Rod Kit, set of 6
      • F-9017-K    Q-FOG SSP-1100 or CCT-1100 20mm (3/4”) Hanging Rod Kit, set of 8

      Other Accessories
      Q-Lab offers a fog collection kit for the Q-FOG tester, which consists of a set of six graduated cylinders, o-rings, and collection funnels.

      Also available is a one-year maintenance parts kit, which consists of eight pump tubes, one air filter, two solution filters elements, and a handy hex wrench.

      Technical Bulletins

      Technical Articles

      Product Brochures

      Specification Bulletins